▶ Testing recalled Infinity cables – outer insulation – YouTube


Video shows how how the Infinity cables prematurely degrade when exposed to high temperatures. Test oven = Ten months at 90 degrees Celsius

via ▶ Testing recalled Infinity cables – outer insulation – YouTube.